4.12 The electrolytic nickel plating process is carried out at a cathodic current density of 4.0 A/dm2 with a current efficiency of 96%. The layer thickness on the parts is 25 microns. Calculate the duration of the process when nickel plating 1 m2 of parts; power consumption at bath voltage 5.0 and voltage loss 10%; (Ni2+).
Additional Information
If you cannot open the file or have any problems, do not rush to leave a negative review! Contact me and I will quickly help you solve the problem. After purchasing, please leave a positive review of the product :)
Related Products
30. Solving a chemistry problem
Seller: Derkach
21. Solving a chemistry problem
Seller: Derkach
50. Solving a chemistry problem
Seller: Derkach
75. Solving a chemistry problem
Seller: Derkach
120. Solving a chemistry problem
Seller: Derkach
124. Solving a chemistry problem
Seller: Derkach
138. Solving a chemistry problem
Seller: Derkach
143. Solving a chemistry problem
Seller: Derkach